Remanent magnetization states (shown as color maps of the horizontal magnetization projection) of various thin films initially saturated in the vertical direction: left image – Py, middle – fcc Co and right – hcp Co.
All films are 20 nm thick and have identical random polycrystalline structures with the average grain size 20 nm.
Magnetocrystalline anisotropy constants are: K
Py = 5 x 10
4 erg/cm
3 (cubic anisotropy),
K
Co,fcc = – 6 x 10
5 erg/cm
3 (cubic anisotropy), K
Co,hcp = 4 x 10
6 erg/cm
3 (uniaxial anisotropy). Lateral size of the area shown on all images is 2 x 5 μ
2 (discretized into 400 x 1000 cells).